Why can not shake hot powder for DTF film clean?

1. There is a problem with the quality of DTF film. Under the same consumables and the same production environment, if you change to another DTF film and the powder sticking problem is improved, one possibility is that the DTF film is of poor quality and unqualified; the other...

Development prospect of heat transfer film

Water-based DTF film, different from oil-based? Which is better?

Suitable for digital transfer printing. The pattern after transfering has the same texture as PU glue, and the hand feeling softer than glue (30~50% softer than the pattern printed with oil-based coating film). Key technology - ink-absorbing release coating (3-in-1 function) can complete the three major needs of ink...

Haiyi DTf film

Haiyi DTf film The surface of the film is dry and clean, and can be easily peeled in the hot, cold and warm conditions. Major advantages: The pattern after ironing is like the texture of PU glue, the tensile resilience is strong and does not deform, and the feel is softer than...

In the process of heat transfer, have you encountered the situation that it is not easy to tear? why it is not easy to peel off?

1. The hot stamping temperature is wrong, it must be adjusted to a suitable temperature. The hot stamping temperature of a pure cotton T-shirt is about 140-160. 2. The pressure of hot stamping is not enough, the pressure of hot stamping should be increased, the greater the pressure, the better...